Vol.25, No.3, 2025, pp. 467–470 |
|
MnFeCoNiCu LEGURE VISOKE ENTROPIJE FORMIRANE EKSPLOZIVNIM NANOŠENJEM SMEŠE PRAŠKA I NAKNADNOM LASERSKOM OBRADOM Igor S. Batraev1
Boris B. Bokhonov3 Marina N. Samodurov1,2
1) Lavrentyev Institute of Hydrodynamics SB RAS, Novosibirsk, RUSSIA I.S. Batraev https://orcid.org/0000-0002-0364-144X ; V.Yu. Ulianitsky https://orcid.org/0000-0002-3538-1486 ; D.V. Dudina https://orcid.org/0000-0003-0010-4638 ; M.N. Samodurova https://orcid.org/0000-0002-1505-1068 2) South Ural State University (National Research University), Chelyabinsk, RUSSIA E.A. Trofimov https://orcid.org/0000-0001-8073-3244 3) Institute of Solid State Chemistry and Mechanochemistry SB RAS, Novosibirsk, RUSSIA T.M. Vidyuk https://orcid.org/0000-0002-6819-8290 ; B.B. Bokhonov https://orcid.org/0000-0002-1729-7731 ; A.V. Ukhina https://orcid.org/0000-0003-1878-0538 4) Khristianovich Institute of Theoretical and Applied Mechanics SB RAS, Novosibirsk, RUSSIA *email: dina1807@gmail.com
|
|
Izvod Formiranje MnFeCoNiCu legure visoke entropije eksplozivnim nanošenjem smeše praška sa naknadnom laserskom obradom se ovde iznosi prvi put. S obzirom da se komponente smeše razlikuju u efikasnosti nanošenja, sastav nanesenog materijala može se razlikovati u odnosu na sirovinski sastav praška. U prevlaci sačinjenoj od ekvimolarne mešavine, koncentracije železa i nikla su znatno veće u odnosu na sirovinski sastav. Sastav sirovinskog praška se reguliše smanjenjem koncentracija nikla i železa kako bi se postigao sastav nanetog sloja u bliskim granicama zahtevanog sastava. Mešavinom 26Mn+11Fe+22Co+13Ni+28Cu (at.%) se formira prevlaka Mn20Fe18Co22Ni18Cu22. Laserska obrada nanetog sloja omogućava stvaranje čvrstih rastvora strukture tipa kubne površinski centrirane rešetke. U prekristalisanom materijalu, međudendritski prostor je obogaćen bakrom. Ključne reči: • legure visoke entropije • prašak • eksplozivno nanošenje • laserska obrada |
|
rad u celosti (1,12 MB) |